info@hxstainlesssteel.com
159-9525-3756
Austenitic steel
316 Stainless Steel Round Bar

316 Stainless Steel Round Bar

Austenitic steel

316 is a brand under American Standard It belongs to stainless steel heat-resisting. corrosion-resisting steel. It is austenitic stainless steel The national standard is 0Cr17Ni12Mo2 It's better than 304 stainless steel In seawater and other media Corrosion resistance is better than 0Cr19Ni9 Mai

PRODUCT INTRODUCTION

316 is a brand under American Standard It belongs to stainless steel heat-resisting. corrosion-resisting steel. It is austenitic stainless steel The national standard is 0Cr17Ni12Mo2 It's better than 304 stainless steel In seawater and other media Corrosion resistance is better than 0Cr19Ni9 Mainly pitting corrosion resistant materials.

                                                                    316 stainless steel round bar

The appearance difference between 316 stainless steel and 304 stainless steel is as follows:

At present, the two most commonly used stainless steels 304316 (or 1.4308,1.4408 corresponding to German / European standards), the main difference between 316 and 304 in chemical composition is that 316 contains Mo, and it is generally recognized that 316 has better corrosion resistance and is more corrosion resistant than 304 in high temperature environment. Therefore, in high temperature environment, engineers generally choose 316 parts.

316 stainless steel round bar chemical composition:

c≤0.08
Si≤1.00
Mn
≤2.00
S≤0.030
P≤0.035
Cr16.00~18.50
Ni10.00~14.00
Mo2.00~3.00

Mechanical properties of 316 stainless steel round bar

Conditional yield strength σ 0.2 (MPa)≥205
Elongation δ 5 (%)≥40
Reduction of area ψ (%)≥60
Hardness≤ 187hb; ≤90HRB; ≤200HV

● heat treatment specification and metallographic structure:

Heat treatment specification: solid solution 1010 ~ 1150 ℃ rapid cooling.

Metallographic structure: the structure is characterized by austenite type.

● delivery status: generally delivered in heat treatment status, and the type of heat treatment is indicated in the contract; If it is not indicated, it shall be delivered without heat treatment




CONTACT FORM

feedbackX